A method for forming a thin film on a substrate layer by layer using plasma enhanced atomic layer deposition is described. The system and the method may use pressure measurements and temperature measurements to determine controlled fracture pressures before the uncontrolled fracture pressure is reached. DBI may be used in addition, or as an alternative, to bit reordering to further minimize the number of bit transitions per bit time. The control part controls the image forming part to perform a deactivation standby operation to stand by for a predetermined time while the image forming part is continuously set in an operating state after the image forming part completes the image forming operation, without querying the higher-order component about an image forming operation to be performed subsequently. Even so, the invention provides at least 15 dB more echo suppression than systems without a sub-band filter bank series coupled with a non-linear processor in each channel. The outer portion is offset from the inner portion and is positioned further away from the other side surface compared to the inner portion.